预防通风管道开裂就这么简单

来源:/     发布时间:2017-05-10  

1、胶水的调制也直接关系到玻镁复合风管在预防开裂表象上的重要性;胶水过稠或过稀都会惹起风管接口开裂,所以在调制的时分必定要把握好稠度。
1, the modulation glue is directly related to the glass fiber and magnesium duct in the prevention of cracking on the importance of representation; glue is too thick or too thin will make the wind pipe interface cracking, so in the modulation of the time bound to grasp consistency.
2、卤水的浓渡过高或过低所致使的风管开裂表象;通常复合风管的制造人员都会把卤水浓度定在一个标准上或是凭觉得来调制卤水的浓度.
2, the brine concentration is too high or too low caused by the wind pipe cracking appearance; usually composite wind pipe manufacturers will put the brine concentration on a standard or on the basis of the concentration of brine
3、夏天在调制卤水的时分由于气温很高所以要把浓度控制在21-23度左右,在初调的时分只需能抵达21 度就能够了,由于卤片消融的时间比照长,等卤片完整消融后再去检验浓度这样比照准确。
In the summer of 3, when the modulation brine temperature is high so the concentration control in 21-23 degrees, in the early hours of just to reach 21 degrees can, because the bittern ablation time by long, such as halogen tablets after ablation to complete this concentration by accurate inspection.
4、冬天的气温较低,所以在调制卤水时应该把浓度控制在25-28度左右,同样在初调的时分浓度应该控制在25度左右等完整化开后再去丈量浓度。
4, the winter temperature is low, so in the modulation of brine should be controlled in the concentration of about 25-28 degrees, the same time at the beginning of the concentration should be controlled at around 25 degrees after the completion of the integrity of the measured concentration.
5、组合风管时应该把胶水调制的稀点,调好后手抓时胶水能自动流出。衔接时的胶水应该调制到和泥灰稠度成比照不能过于太稀。
5, combined wind pipe should put some glue diluted modulation, good hand grasping glue can automatically flow. The glue should be glued to the consistency of the paste and not too thin.
本文由山东通风管道加工厂家为您提供,我们的网站是:/ 我们将以全心全意的热情为您提供更的服务,欢迎您的访问!
This article by the Shandong ventilation pipe processing factory to provide you, our website is: / we will be dedicated to provide you with the best quality service, welcome your visit!